BOPP White 60/Acrylic C-03/PET30
Uso:
- Minimum labeling temp: 5℃
- Service temp: -20℃~80℃ (24h after labeling)
- Suitable for application of daily chemical label & food label.
- Must test to confirm if used in small bottle label (diameter smaller than 30mm).
- Not recommended for bottles with irregular surfaces or extruded bottles. Foamed structural facestock for economical applications, such as label peeling and high-speed large-angle bending, may develop fine cracks. When testing the adhesion strength of inks or coatings with 3M 600/810 tapes, there is a risk of film rupture and delamination.
Fabricado por Youhua. Vendido en EE. UU. por Adwins International.
Detalle
Aplicación
Fulfill the requirement of ROHS, REACH, VOC
Minimum labeling temp: 5℃
Service temp: -20℃~80℃ (24h after labeling)
Suitable for application of daily chemical label & food label.
Must test to confirm if used in small bottle label (diameter smaller than 30mm).
Not recommended for bottles with irregular surfaces or extruded bottles. Foamed structural facestock for economical applications, such as label peeling and high-speed large-angle bending, may develop fine cracks. When testing the adhesion strength of inks or coatings with 3M 600/810 tapes, there is a risk of film rupture and delamination.
Impresión y procesamiento
With special treatment coating, can be used in relief printing, flexography printing, gravure printing, screen printing and varieties of printing methods. Suitable for UV ink and water-based ink.
Control the viscosity of print ink, high contractility bring label crimp, causing the label detach from release paper or warp from label object.
Sharp special die-cut knife for film is recommended especially platen die cut.
PET liner is well suited for high-speed die cutting and labeling. The printed labels should avoid contact with high-concentration alcohol, isopropyl alcohol, benzene, and oxidizing liquids such as H2O2 as much as possible to prevent the separation of ink from the coating or substrate.
Plazo y condiciones de almacenamiento
From date of manufacture: 12 months
Storage conditions: 23±2℃ & relative humidity 50±5%.
Prolonged storage outside these conditions might reduce the shelf life.
| Indicador | Parámetro | Unidad | Método |
|---|---|---|---|
| Substance | 45±5% | g/㎡ | ISO 536 |
| Caliper | 60±5% | μm | ISO 534 |
| Indicador | Parámetro | Unidad | Método |
|---|---|---|---|
| Initial Tack | ≥7.5 | N | FTM9,ss |
| 90°Peel Adhesion (20min) | ≥4.5 | N/25mm | FTM2,ss |
| Shear | ≥20 | hours | FTM8,ss |
| Indicador | Parámetro | Unidad | Método |
|---|---|---|---|
| Caliper | 30±5% | μm | ISO 534 |
Declaración
Todas las declaraciones, la información técnica y las recomendaciones se basan en pruebas que se consideran confiables, pero no constituyen una garantía. El cliente debe probar todos los productos vendidos en el entorno de uso final para confirmar que cumplen con los requisitos de dicho entorno y para determinar qué materiales comprar. Nos reservamos el derecho de interpretación final.